TY - JOUR AU1 - SHIGAKI, Ichiro AU2 - SAWADA, Mineo AU3 - GENNAI, Norio AU4 - TI - Increase in low-temperature reduction degradation of iron ore sinter due to hematite-alumina solid solution and columnar calcium ferrite. JF - Transactions of the Iron and Steel Institute of Japan DO - 10.2355/isijinternational1966.26.503 DA - 1986-01-01 UR - https://www.deepdyve.com/lp/unpaywall/increase-in-low-temperature-reduction-degradation-of-iron-ore-sinter-uPEJ0v0mOq DP - DeepDyve ER -